Vol 5, No 4 (2014) | Ab-initio study of Re and Ru effect on stability of TCP nanoparticles in Ni-based superalloys | Abstract PDF (Eng) similar documents |
N. I. Medvedeva, A. L. Ivanovskii | ||
"... Modern nickel-based superalloys contain high concentrations of rhenium that allows the improvement ..." | ||
1 - 1 of 1 Items |
Search tips:
- Search terms are case-insensitive
- Common words are ignored
- By default articles containing any term in the query are returned (i.e., OR is implied)
- Make sure that a word exists in an article by prefixing it with +; e.g., +journal +access scholarly academic
- Combine multiple words with AND to find articles containing all terms; e.g., education AND research
- Exclude a word by prefixing it with - or NOT; e.g., online -politics or online NOT politics
- Search for an exact phrase by putting it in quotes; e.g., "open access publishing". Hint: Quoting Chinese or Japanese words will help you to find exact word matches in mixed-language fields, e.g. "中国".
- Use parentheses to create more complex queries; e.g., archive ((journal AND conference) NOT theses)